Question

What NDE does each API 653 tank repair need?

API 653 Section 12.1 sets the examination for each kind of repair, on top of API 650 Section 8, which governs the methods, examiner qualification and acceptance. One rule covers every repair: each new weld, and every cavity left by gouging or grinding, is examined visually over its full length (12.1.1.5). The rest depends on what was repaired.

Nozzles, reinforcing plates and hot taps (12.1.2)

  • Adding a reinforcing plate to an unreinforced nozzle, or adding a hot tap: ultrasonic examination of the shell plate for laminations in the immediate area affected.
  • Removing an old reinforcing plate: magnetic particle or penetrant examination of the cavities left by gouging or grinding out its welds.
  • Completed nozzle neck-to-shell, reinforcing plate-to-shell and reinforcing plate-to-neck welds: magnetic particle or penetrant. For a hot tap on shell plate of unknown toughness, consider more (fluorescent magnetic particle or ultrasonic).
  • Stress-relieved assemblies: magnetic particle or penetrant after stress relief and before the hydrotest.
  • New or altered reinforcing plates also get an air leak test (12.4).

Weld defect repairs (12.1.3)

  • The cavity left by removing the defect: magnetic particle or penetrant.
  • A completed repair of a butt weld: radiography or ultrasonic examination over its full length.
  • A completed repair of a fillet weld: the appropriate method over its full length.

Attachments to the shell (12.1.4)

Welds of permanent attachments, and areas where temporary attachments were removed and ground off, are examined visually. On API 650 Group IV, IVA, V or VI material, or when the material group cannot be established, they also get magnetic particle examination (penetrant at the purchaser’s option).

Shell plate (12.1.5, 12.1.8, 12.2)

  • New shell butt welds: radiography. Welds that join existing plate get more than new-to-new welds; see the page on new versus existing shell welds.
  • Corrosion repaired by weld metal deposit: visual before and magnetic particle (or penetrant) after.
  • Lap-welded shell patches: visual plus magnetic particle or penetrant on the attachment welds.

Shell-to-bottom weld (12.1.6)

  • New welding on the shell-to-bottom joint: a right-angle vacuum box over the full length, or light diesel oil; the first pass is also checked with oil on the opposite side, left to stand at least four hours.
  • The alternative: visual on the cleaned initial passes, then an air test between the inside and outside welds with a soap film on both.
  • Under a new welded-on bottom patch plate: visual plus magnetic particle or penetrant on the existing shell-to-bottom weld for the patch length and six inches beyond each side, before the patch goes on.

Bottom (12.1.7)

  • All new bottom welds, patch plate welds, areas restored by welding and repaired defect welds: visual, then one of the API 650 bottom leak tests: vacuum box, tracer gas, or water pumped under the bottom. Leaks are repaired and retested.
  • A patch plate in the critical zone: root and final pass visual plus magnetic particle or penetrant over the full length.
  • Bottom plate repaired by welding: magnetic particle or penetrant, plus a vacuum box or tracer gas test.

Roofs and friction studs (12.1.9 to 12.1.11)

Fixed roof joints and repairs follow API 650. A floating roof repair gets a visual examination from the top and bottom, then an air, vacuum box, penetrating oil, tracer gas or other leak test of the repaired welds, or a flotation test instead. Friction-welded studs are examined visually and torque tested.

When a hydrotest is skipped

A major repair taken through the 12.3.3 path instead of a hydrotest adds examinations: full radiography of new shell butt welds, back-gouged root and completed-weld checks on nozzle welds plus ultrasonic, magnetic particle or penetrant after the root and final pass on critical-zone bottom repairs (and ultrasonic on annular butt welds), and visual plus magnetic particle or penetrant at three stages on shell-to-bottom weld repairs.

Repair NDE in TankForge

Each repair on the repair log carries its own examination results (visual, penetrant, magnetic particle, ultrasonic, radiography), the penetrant steps before and after welding, and the leak tests. The draft report carries the repair tables and the NDE forms; your certified inspector reviews and signs.