MFL vs UT for a tank floor: which one, and when?
Most tank floors get both. API 653 clause 4.4.4 says MFL (magnetic flux leakage) tools are commonly used along with UT (ultrasonic thickness) tools to examine tank bottoms, and that UT is often used to confirm and further size what the MFL scan found. MFL covers the floor quickly and finds where the metal loss is; UT tells you how thick the plate is at that spot.
What each method gives you
- MFL: a scanner rolled across the plates flags metal loss on either side of the plate, including soil-side corrosion you cannot see. It screens large areas fast, but an indication is a signal, not a measured thickness.
- UT: a thickness reading at a point, or along a scan, from the top side. It is exact where it is taken but slow to cover a whole floor.
- In practice, scanners usually cannot reach right up to the shell, into corners or around obstructions, so those areas, including much of the critical zone, are often covered with UT or a smaller hand scanner.
Does MFL replace UT?
Not as a rule. Clause 4.4.4 says UT is often used to confirm and quantify MFL data, but may not be required depending on the specific procedure and application. Whether an MFL call needs UT prove-up is set by the qualified procedure and the owner’s requirements, and the report lists each method used and its results (clause 6.9.2 h).
How are MFL indications proved up?
In practice, each indication is marked on the plate, then sized from the top side: UT for remaining thickness where the loss is soil side, and a pit depth measurement where it is product side. The least remaining thickness found, after any repairs, goes into the bottom minimum remaining thickness calculation of clause 4.4.5.1.
The MFL threshold
For a bottom scanned by MFL and without effective cathodic protection, the soil-side rate is worked from the lesser of the MFL threshold and the thinnest unrepaired corrosion (clause 4.4.5.1, NOTE 1). The MFL threshold is the least remaining thickness the scan must detect, and the tank owner sets it beforehand from the interval wanted. A lower threshold means the scan only has to find deeper loss. Plate with no indication is then assumed to be as thin as the threshold, so the interval it supports is shorter.
Who can do it
Data quality from both methods depends on the people, the equipment and the procedure (clause 4.4.4). UT thickness examiners need ASNT UT Level II full or limited certification under an approved procedure (clause 12.1.1.4). For MFL, clause 12.1.1.6 points to API 575, Annex D for guidance on qualifying personnel and procedures, and leaves the specific requirements to the owner/operator. Annex G of API 653 is left blank in Addendum 4.
MFL in TankForge
In TankForge the inspector can mark MFL hits, MFL indications and MFL repair-area boxes on the floor drawing; it does not import MFL scan files.
Also asked as
MFL floor scan vs UT: what is the difference?
An MFL floor scan screens the whole bottom quickly for metal loss on either side of the plate; UT measures the actual thickness at a point. The scan finds where to look, and UT sizes what it found.
Does MFL replace UT on a tank bottom?
Not as a rule. API 653 clause 4.4.4 says UT is often used to confirm and quantify MFL data, but may not be required depending on the specific procedure and application.
How are MFL indications proved up?
In practice, each indication is located on the plate and sized from the top side: UT for remaining thickness on soil-side loss, a pit depth measurement on product-side pits. The least remaining thickness feeds the bottom calculation of clause 4.4.5.1.
TankForge is API 653 inspection software built by a working API 653 inspector. Draft report. Your certified inspector reviews and signs.